Problem: Powder depositing on an object

Cause Remedies
Total air setting too low. The ideal air volume should be in the region of 4 - 5 Nm3.
Fine grain powder / powder with poor flow properties. Using a powder hopper with fluidizing air, and vibration will help.
Short term, high compressed air consumption can cause pressure fluctuations. Fitting a larger compressed air reservoir directly before a high
air consumption position will solve this problem.
A too small cross-section or too small radius in the powder hose line up. Radius must be at least 150 - 200 mm.
A poor ratio between fresh powder  and recovered powder. Use an automatic fresh powder feed.
Too high / low output Adapt to the coating parameters.
Contaminated injectors Use an automatic fresh powder feed.